A-8521 compatibilizer for LDPE, EVA and polyolefin blends

A-8521 is documented as form not stated in source tds for LDPE / EVA / PO / Fillers and polymer blends. The source TDS lists 2-4% and positions the grade for interfacial adhesion, blend compatibility and split-resistance improvement.

A-8521 Form not stated in source TDS
Form not stated in source TDS
Recommended materialsLDPE / EVA / PO / Fillers and polymer blends
Starting dosage2-4%
Form and packForm not stated in source TDS
25 kg paper-poly pouch
TDS-derived technical profile

Key values listed for A-8521

The following technical values are taken from the current TDS to support grade selection and initial formulation work.

PropertyListed value
Listed dosage2-4%
Density0.9 g/cm3
Melt flow rate0.6 g/10 min
Hardness68 Shore A
Melting point108-126°C
Elongation at break800%
Selection direction

What this grade is positioned to support

  • Polymer-blend compatibility
  • Interfacial adhesion support
  • Toughness and split-resistance evaluation
Trial workflow

How to prepare the first evaluation

  1. 01

    Blend A-8521 with the selected resin for 5-8 minutes.

  2. 02

    Proceed by extrusion, injection molding or blow molding after uniform mixing.

  3. 03

    Evaluate the target property on matched control and modified samples.