Back to MAPP compatibilizerMAPP compatibilizer

A-8524

MAPP compatibilizer for PP, polymers and fillers

A 100%-active MAPP grade documented to improve compatibility and interfacial binding between PP, other polymers, fillers and materials.

A-8524 Granule
Granule
Recommended materialsPP / Polymer blends / Filled compounds
Starting dosage2-4% listed range
Form and packGranule
25 kg paper-poly pouch
TDS-derived technical profile

Key values listed for A-8524

The following technical values are taken from the current TDS to support grade selection and initial formulation work.

PropertyListed value
Effective substance content100%
Density0.9 g/cm³
Melt flow rate0.6 g/10 min
Hardness78 Shore A
Vicat softening temperature60-70°C
Ash0%
Selection direction

What this grade is positioned to support

  • PP and filler interface support
  • Polymer-blend compatibility
  • Binding-strength and impact-retention evaluation
Trial workflow

How to prepare the first evaluation

  1. 01

    Blend A-8524 with the selected resin/filler system for 5-8 minutes.

  2. 02

    Keep blend ratio and filler treatment constant in the control.

  3. 03

    Proceed by extrusion, injection molding or blow molding after uniform mixing.

Technical documentation

Current TDS and application guidance

Source file: a-8524-tds.pdf. No compatibilizer is universal; confirm both polymer grades and the filler surface chemistry. Measure interface-dependent properties on the final blend.

Request current TDS